Why insufficient transparency of stretch winding film
Source:Why insufficient transparency of stretch winding filmTime:2019-03-25Visitors:
We often look at the logistics company's use of stretch-wound film, stretch-wrap film by means of the film's superior winding force and retractability, the product is compactly and fixedly bundled into a unit, even in the unfavorable environment, the product does not have any Loose and separate, with no sharp edges and stickiness to avoid damage.
1. The rubber roller or scraper is defective, and a certain point cannot be pressed, forming a neutral position and being opaque.
2. The inlet temperature of the drying tunnel is too high or there is no temperature gradient. The inlet temperature is too high and the drying is too fast, so that the solvent on the surface of the glue layer evaporates rapidly, the surface is crusted, and then when the heat penetrates into the inside of the glue layer, the film is under the film. The solvent vaporizes and breaks through the film to form a ring like a volcanic vent. One turn and one turn makes the wound film opaque.
3. There is too much dust in the air of the manufacturer's environment. There is dust in the hot air blown into the drying tunnel after the glue is applied. Adhesive on the surface of the adhesive layer, sandwiched between the two base films during compounding, with many small dots, resulting in opacity.
4. No rubber roller or rubber roller is not clean.
5. The amount of glue on the stretch wrapping film is insufficient, there is a blank space, and there is a small air bubble, which causes the spot or opacity. The amount of glue should be checked to make it sufficient and uniform.
1. The rubber roller or scraper is defective, and a certain point cannot be pressed, forming a neutral position and being opaque.
2. The inlet temperature of the drying tunnel is too high or there is no temperature gradient. The inlet temperature is too high and the drying is too fast, so that the solvent on the surface of the glue layer evaporates rapidly, the surface is crusted, and then when the heat penetrates into the inside of the glue layer, the film is under the film. The solvent vaporizes and breaks through the film to form a ring like a volcanic vent. One turn and one turn makes the wound film opaque.
3. There is too much dust in the air of the manufacturer's environment. There is dust in the hot air blown into the drying tunnel after the glue is applied. Adhesive on the surface of the adhesive layer, sandwiched between the two base films during compounding, with many small dots, resulting in opacity.
4. No rubber roller or rubber roller is not clean.
5. The amount of glue on the stretch wrapping film is insufficient, there is a blank space, and there is a small air bubble, which causes the spot or opacity. The amount of glue should be checked to make it sufficient and uniform.

Recommended Products
Ranked in the same article
- how to use the stretch film technology to r
- How can we get detailed price list?
- Five common quality problems of PE protecti
- Plastic film degradation
- Gauge to Micron and Millimetre Conversion G
- How to guarantee punctual shipment for our
- What is the difference between stretch film
- Stretch film temperature requirements
- Testing the permeability of stretch film
- Electrical wire film VS electrostatic film
- The elastic characteristics of plastic film
Latest news articles
- The advantages of stretch film on packaging
- A brief look at the competitive market of s
- What Size is a Shrink Film?
- Advantages of stretch wrapping film on pack
- PE stretch film development market
- Bundling Stretch Film: Optimize Your Packag
- Choosing the Right Dispenser for Bundling S
- The characteristics of the stretched film q
- How stretch film works
- 5 Major Benefits of RoHS-Certified Electric
- Application field of stretch wrapping film